Projected plaster with a high composition of perlite that has exceptional qualities such as: An increase in retention
of water, increased performance thanks to its lower density, the screeding, cutting and plastering operations are easily carried out due to its slow and progressive setting and hardening thanks to the fact that perlite is included in its composition.
This material has a high coefficient of thermal conductivity and, given its porous structure, provides good acoustic and thermal insulation, protection against low temperatures and against fire.
Water/Plaster Ratio | 10–11 litres per bag |
Powder density | <800 kg/m3 |
Initial set time | >120 min |
Shore Hardness C | ≥65 |
Compressive strength | ≥2 N/mm2 |
Bending resistance | ≥1 N/mm2 |
Output | 1.5 m2/sack/cm thickness ±5% |
Note: Workability can vary depending on water/plaster, proportions, temperature, water pH, base type, mixing velocity and time.